Characteristics of biofilm-induced degradation at resin–dentin interfaces using multiple combinations of adhesives and resins

作者
通讯作者Zhou,Yuan
发表日期
2021
DOI
发表期刊
ISSN
0109-5641
卷号37页码:1260-1272
摘要
Objective: We aimed to evaluate morphological, mechanical and chemical characteristics at resin–dentin interfaces using multiple combinations of adhesives and resins after a short-term biofilm-induced degradation. Methods: Cervical cavities were prepared in bovine incisors, treated by Clearfil SE Bond 2 (SE) or FL-Bond II (FL), restored by Clearfil Majesty ES Flow (ES) or Beautifil Flow Plus (BFP) and grouped into SE-ES, SE-BFP, FL-ES and FL-BFP. After biofilm challenge, interfacial gaps and dentin wall lesions were examined by optical coherence tomography (OCT). Gap depth (GD), gap pattern scale (GPS) and dentin wall lesion depth (WLD) were evaluated from confocal laser scanning microscope. Microhardness of dentin lesions was measured with a Vickers microhardness tester. Chemical elements in resins and dentin wall lesions were analyzed by scanning electron microscopy and energy dispersive X-ray spectrometry (SEM/EDS). Morphological structures of interfacial gaps were observed by SEM. Results: OCT could detect adhesive-dentin-bonded and adhesive-dentin-debonded gaps. SE-containing groups showed significantly lower GPS than FL-containing groups. FL-BFP showed significantly lower WLD than FL-ES. Microhardness of dentin wall lesions was higher than that of outer lesions and they showed significant differences in FL-BFP. SE-BFP showed a lower GPS curve and higher intensities of Ca and P in the upper half of dentin wall lesions than other groups. From SEM, microgaps between filler and matrix, break and loss of matrix, separation of adhesive matrix with hybrid layer occurred at interfacial gaps. Significance: The morphological, mechanical and chemical characteristics of resin–dentin interfacial degradation depend on the component and chemistry of restorative materials.
关键词
相关链接[Scopus记录]
收录类别
SCI ; EI
语种
英语
学校署名
其他
WOS记录号
WOS:000675411800009
EI入藏号
20211910320642
EI主题词
Biofilms ; Chemical analysis ; Chemical elements ; Degradation ; Mammals ; Microhardness ; Optical tomography ; Resins ; Scanning electron microscopy
EI分类号
Biomaterials (including synthetics):462.5 ; Optical Devices and Systems:741.3 ; Chemical Reactions:802.2 ; Chemical Products Generally:804 ; Organic Polymers:815.1.1 ; Materials Science:951
ESI学科分类
CLINICAL MEDICINE
Scopus记录号
2-s2.0-85105283165
来源库
Scopus
引用统计
被引频次[WOS]:3
成果类型期刊论文
条目标识符http://sustech.caswiz.com/handle/2SGJ60CL/228519
专题工学院_电子与电气工程系
作者单位
1.Laboratory of Molecular and Preventive Dentistry,Department of Preventive Dentistry,Shanghai Ninth People's Hospital,Shanghai Jiao Tong University School of Medicine,Shanghai,639 Zhizaoju Road, Huangpu District,200011,China
2.Department of Cariology and Operative Dentistry,Graduate School of Medical and Dental Sciences,Tokyo Medical and Dental University,Tokyo,1-5-45 Yushima, Bunkyo-ku,113-8549,Japan
3.Endowed Department of International Oral Health Science (affiliated with Department of Translational Research),School of Dental Medicine,Tsurumi University,Yokohama-shi,2-1-3 Tsurumi, Tsurumi-ku,230-0063,Japan
4.Department of Operative Dentistry,Graduate School of Medicine,Dentistry and Pharmaceutical Sciences,Okayama University,Okayama,2-5-1 Shikata-cho, Kita-ku,700-8525,Japan
5.Biomimetics Biomaterials Biophotonics & Technology Laboratory,Department of Restorative Dentistry,University of Washington School of Dentistry,Seattle,1959 NE Pacific Street,98195-7456,United States
6.Department of Electrical and Electronic Engineering,Southern University of Science and Technology,Shenzhen,1088 Xueyuan Ave, Nanshan District,518055,China
推荐引用方式
GB/T 7714
Zhou,Yuan,Matin,Khairul,Shimada,Yasushi,等. Characteristics of biofilm-induced degradation at resin–dentin interfaces using multiple combinations of adhesives and resins[J]. DENTAL MATERIALS,2021,37:1260-1272.
APA
Zhou,Yuan.,Matin,Khairul.,Shimada,Yasushi.,Sadr,Alireza.,Wang,Guoqing.,...&Feng,Xiping.(2021).Characteristics of biofilm-induced degradation at resin–dentin interfaces using multiple combinations of adhesives and resins.DENTAL MATERIALS,37,1260-1272.
MLA
Zhou,Yuan,et al."Characteristics of biofilm-induced degradation at resin–dentin interfaces using multiple combinations of adhesives and resins".DENTAL MATERIALS 37(2021):1260-1272.
条目包含的文件
条目无相关文件。
个性服务
原文链接
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
导出为Excel格式
导出为Csv格式
Altmetrics Score
谷歌学术
谷歌学术中相似的文章
[Zhou,Yuan]的文章
[Matin,Khairul]的文章
[Shimada,Yasushi]的文章
百度学术
百度学术中相似的文章
[Zhou,Yuan]的文章
[Matin,Khairul]的文章
[Shimada,Yasushi]的文章
必应学术
必应学术中相似的文章
[Zhou,Yuan]的文章
[Matin,Khairul]的文章
[Shimada,Yasushi]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
[发表评论/异议/意见]
暂无评论

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。